[rp-ml] SLA prototype

From: Kiran <office_mail_3_at_yahoo.co.in>
Date: Sat Sep 25 2004 - 13:02:12 EEST

 
Hello Friends,
 
I am facing problem while making a silicon rubber(Additional cure RTV) mold using SLA master.The rubber surface which is in contact with the master surface will remain tacky even after painting or applying a surfacer coat on the SLA surface and cure it at a room temperature.
 
Can any one tell us how to over come with this problem.
 
 Regards
Vinod Kumar
India.