Hosein,

Z-Corp models are suitable for sand casting - Model will need to be
infiltrated with durable hard material.

Z-Corp doesn't recommend pouring any metals above 2000 deg F or 1100 deg C
with Z-Cast material. Non ferrous only.

Jim Pike