I'm looking to produce some bronzes.

Can anyone talk definitively on the issues regarding going with a
Quickcast positive and a rubber mold as opposed to going directly to wax?

I've done both the ZCorp direct to metal (super) and the sintered bronze
processes (super) but I'd like to get a handle on these relatively more
traditional methods.

Also happy to hear from vendors or those with access to these processes.

On or off-list.

Thanks,

Jonathan

-- 
Universal Joint Design Associates
Development + Design + Construction
http://www.universaljointdesign.com
[ bLOG ] on digital tools, rapid prototyping technologies and the fabrication of free-form structure.
Jonathan Chertok. Principal 
Austin, Texas  1 512 407 9628
This e-mail and its attachments may contain confidential information. It
is intended solely for the use of the addressee(s) named herein. Any use
of the information contained herein by other persons is prohibited. If
you have received this e-mail by mistake, please immediately notify the
sender (via the phone number above or email) and permanently delete the original as well as any copy thereof.
Do not use any files or other data, via ftp or other means, without subsequent permission in writing.
UJDA does not accept any liability for the contents of this
e-mail or its attachments. 

Received on Mon Apr 07 19:23:47 2008

This archive was generated by hypermail 2.1.8 : Tue Jan 06 2009 - 15:48:27 EET