From: ProtoCall (parts@protocallonline.com)
Date: Tue Mar 27 2007 - 22:04:52 EEST
Hi All,
Does anyone have experience running this material Innovative polymers
VA-300) in silicone tools/molds?
We ran some and it dried up our molds in about 7 shots.
Really hoping to find some help on this one!!!
Either with silicone recommendations, pointers or leads to shops that can
run lager parts in this material.
Doug Johnson
ProtoCall, LLC
262-446-3104