Hi All,
Does anyone have the correct thermal post-cure process for SI-40 resin?
I believe it is this, but please concur or edit if it's off the mark:
- ramp-up from room temperature to 80C over 2 hours.
- hold for 2 hours at 80C
- ramp back down to room temperature over at least 2 hours.
Thanks!
Ron DeFonce
Received on Tue Apr 04 18:53:39 2006