I'm not sure I understand your exact question.

Machine layer thickness? You can alter your layer thickness from 0.003" per
layer to roughly 0.010" per layer. I think the distance from the roller to
the base plate is roughly 0.060".

Specific Heat. . . Hmm. If you are talking part heater setpoint, that will
vary from platform to platform. We generally run a setpoint of 150-160 for
Duraform products and 90-110 for Laserform.
*********************************************
David K. Leigh (254)933-1000
Harvest Technologies fax(254)298-0125
Rapid Prototyping Services dkleigh@harvest-tech.com

  -----Original Message-----
  From: owner-rp-ml@rapid.lpt.fi [mailto:owner-rp-ml@rapid.lpt.fi]On Behalf
Of nambi arun rajan
  Sent: Wednesday, April 14, 2004 5:41 AM
  To: rp-ml@rapid.lpt.fi
  Subject: Details need for SLS

  Hi All,

  I want the following details for DTM SLS 2500Plus machine.

  1. Machine Layer Thickness (It is different from Powder Layer Thickness)
  2. Specific Heat of Material( LaserForm, DuraForm PA & GF).

  Can anybody provide me these details.

  Thanks

  With Regards

  P.Nambi Arun Rajan