Dear all,
We need to increase hardness and to eliminate the porosity of the SLS
parts.
I think i've read before on this list, that there is one process of
infiltration/coating to achieve this objective..
There's someone that can help me on this subject.
Best regards,
Sergio Martins
-- *********************************************************** Sérgio Martins mailto:s.martins@distrim2.pt DISTRIM 2 - Indústria, Investigação e Desenvolvimento, lda http://www.distrim2.pt *********************************************************** Some Men see things as they are and say why, I dream things as they never were and say why not.