Re: SLA material question

From: Jean-Marc Boéchat (jean-marc.boechat@mimsystems.com)
Date: Fri Oct 11 2002 - 10:06:55 EEST


Hi Doug:

I think the polypro choice was questionable to say the least. I would go
with filled or unfilled polyamid for a start but there are other choices
like POM or polycarbonate depending on the the other conditions and
price constrains.

Hope this helps.

Jean-Marc

parts wrote:

> Hi All,I have made several small turbine fans for one of my
> customers.He spins them up to 130,000 RPM.The SLA parts behave better
> than the injection molded talc filled polypro parts.He wants to know
> if there is an injection moldable material that has the same
> properties as the 10120 SLA resin.Doug
> ProtoCall, LLC <?xml:namespace prefix = u6 />
>
> 507 West College Avenue<?xml:namespace prefix = o ns =
> "urn:schemas-microsoft-com:office:office" />
>
> Waukesha, WI 53186-4501
>
> 262.446.3104
>
> 262.896.8945 fax
>
> 414.915.0036 cell
>
> www.protocallonline.com
>
> [Image]
>
> parts@protocallonline.com
>

--
Jean-Marc Boéchat               email:
jean-marc.boechat@nafof.mimsystems.com
MIM Systems Ltd                 phone:+4126 430 08 08  fax: +4126 430 08
09
Swiss Branch office               website: www.mimsystems.com
P.O. Box
CH- 1723 Marly 2
Switzerland                     "when things go wrong, don't go with
them!"

Please remove the nafof in my e-mail address before use! Disclaimer: "I speak for myself only, it's hard enough!"

For more information about the rp-ml, see http://rapid.lpt.fi/rp-ml/



This archive was generated by hypermail 2.1.4 : Tue Jan 21 2003 - 20:14:25 EET