RE: Plating of RP parts

From: Groh, Doug (DGroh@PGKServices.com)
Date: Fri May 04 2001 - 16:03:49 EEST


Contact Vacuum Ornametal in Romulus Michigan (home of the Dtroit
Metropolitan Airport). Ask for Frank Chester. The part will show any flaws,
Surface texture etc. It is best if the part is SLA (homogenous) because it
does see some heat. Different materials will heat at different rates causing
some variance in surface if you patch with foreign materials. They can do a
metalized surface in a gold or silver.
The phone number is 734-941-9100

Doug Groh
Director APDS
PGK Engineering, Inc.
185 Elmwood
Troy, MI, 48084

248-577-5227 xt 227
248-577-9869 fax
248-310-6198 cell

-----Original Message-----
From: rees [mailto:x@michaelrees.com]
Sent: Thursday, May 03, 2001 11:00 PM
To: dgroh@pgkengineering.com
Cc: rp-ml; Marc_D_Karnik@email.whirlpool.com
Subject: Re: Plating of RP parts

Here Here!! I seconed that !! rees

"Spielman, Roger L" wrote:

> Management??????
>
> Krylon #1701 Bright Gold
>
> > ----------
> > From:
> >
Marc_D_Karnik@email.whirlpool.com[SMTP:Marc_D_Karnik@email.whirlpool.com]
> > Sent: Thursday, May 03, 2001 12:11 PM
> > To: rp-ml@ltk.hut.fi
> > Subject: Plating of RP parts
> >
> >
> > Does anyone know of a source for gold plating SLS Duraform parts?
> >
> > To ward off the inevitable questions, yes it is for a part to be
> > presented to senior managment.
> >
> > Thanks,
> >
> > Marc Karnik
> >
> > Modelmaker
> > Whirlpool Corp.
> >
> > For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/
> >
>
> For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/

For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/

For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/



This archive was generated by hypermail 2.1.2 : Fri Jan 04 2002 - 09:57:13 EET