Gabe,
Polane is a 3 component polyurethane paint. I believe you can get it from
Sherwin Williams, automotive division. Be careful, it is very toxic and a
bit hard to work with
Rick Harrington
At 07:39 PM 10/29/98 -0700, you wrote:
> I have a client that wants to SLA a part and have it painted for a show
>they are going to. While we have done this many times before, they want a
>specific paint I have never heard of before. It is called a POLANE paint. I
>am wondering if anyone has heard of this kind of paint and if it would
>"destroy" or "eat at" an SLA? Thanks in advance.
>
>--
>Gabe Clark gabe.clark@sdaa.com
>Rapid Prototype Manager (801)-328-8220
>Solid Design & Analysis www.sdaa.com
>
>For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/
>
>
Rick Harrington
Harrington Product Development Center
"Bringing it all Together"
Your partners in product development solutions
Phone: (513)482-4700 Ext.3004
Fax: (513)482-4706
Toll Free: (800)482-2240 Ext 3004
Alpha Numeric Pager (800)393-2834
FTP Site: ftp.harringtonpdc.com
E Mail To: rharrington@harringtonpdc.com
Home Page: http://www.harringtonpdc.com
Snail Mail to:
Richard Harrington
Harrington Product Development Center
1756 Tennessee Avenue
Cincinnati, Ohio 45229
For more information about the rp-ml, see http://ltk.hut.fi/rp-ml/
This archive was generated by hypermail 2.1.2 : Tue Jun 05 2001 - 22:47:04 EEST