Hi David Alons.
I think you are very sensible to the epoxy resin. Some people are, and the
simptomatology can apear long time after being ini contact with it.
We use SterEOSmax 600. (600*600*450 mmm).
After laser lighting our machine waits 8 seconds, then it lights the part and
then it waits 8 seconds again. Then it starts a new layer. The recoater runs
at 40 mm per second, and only recoats the part to be illuminated.
See you David !
Miquel Angel Garrido
Joanot Martínez-Mora
Lucas Grijander de la Pradera
Pedro Pedro Chu Chú
EPSA
Spain (Barcelona)