Exactomer 2202

From: David Susaraba (das@depuy.com)
Date: Wed Jan 24 1996 - 21:44:49 EET


Exactomer users,
We recently switched one of our SLA-250s over to Exactomer's 2202 resin.
Since then we have had trouble with flat down facing surfaces building
quickcast parts coming out waffled or wavy. Compared to our other 250 that
is using Ciba's 5170 resin the surface is terrible. Any suggestions would
be greatly appreciated. Thanks.

David Susaraba
DePuy Orthopaedics